I'm using 'Extreme Power' brand (from Hobby Lobby- I think they're the equivalent of ""Bob Smith brand"" which is from Hobby ToWn)
I've laid down a bead of thick (the yaller bottle, yah?) glue, mebbe 1/4" thick X 3"long, and it's taking f o r e v e r to cure.
(the medium glue is acting the same way).
It's been TEN hours and counting....??! The bond kinda flexes, not what I want to sand, yet...(it's kinda like how old Testor's orange could be, with a bad, high solvent content tube).
I washed the kit parts, the plastic is nothing exotic, I sanded the surfaces slightly to get more 'tooth'....SheeeSH!
ONliest thing I can figger is we got 45% humidity in my country part of Texas City, right now, and there's not enough water to activate the ?ester?
I could use 'zip kicker' cyano activator, but kinda hate to go that far for a teeny little joint. (glad I learnt to glue small areas at a time, over the years, or this would be worser!)
OH, and please, NO solvent glue recomendations...I got some of that, but now prefer cyano glue due to smell/headache hassles, Thanks! (also, I'm just weirded out by this odd non-reaction)

Any Ideas, Out There, Ya'll?